The melting point of the alloy is only 143 ℃, and the wettability is good. While ensuring the requirements of the low-temperature solder paste processing, the problem of poor reliability of the currently commonly used low-temperature solder is fundamentally solved. Compared with earlier Sn42/Bi58 solder joints, the fatigue impact strength is 8.1 times higher, and nearly 2.1 times higher than Sn/Bi35/Ag1 alloys. It is very suitable for flexible light bar welding.
Element |
Sn42Bi58,Sn55Bi35Ag1.0,Sn60Bi35Ag0.5 etc. |
Port |
Qingdao, Shanghai, Tianjin, Shenzhen, etc. |
Certificate |
ISO, etc. |
Payment method |
T/T,Western Union,L/C,etc. |
Package |
Standard export packaging or as required. |
Application |
It can be used as a coating material and has a wide range of applications in food, machinery, electrical appliances, automobiles, aerospace and other industrial sectors. |